Posted by Murddoc on March 20, 2001 at 18:07:08:
In Reply to: Re: What is the difference? posted by MHK on March 20, 2001 at 17:37:17:
In addition to the above it also speaks to a mindset and an approach.. Why worry about figuring out what steel tank ( ie; chromoly -v- galvanized -v- pressed) and the various bouyancy characteristics??? Why not avoid the problem to begin with???
That is why I use the Steel 95 whenever possible. To avoid having to mess with my weights.
We also want to emphasis the potential for a C02 buildup as you are working hard to get to the surface..
I still do not see the difference between having a heavy tank and a little lead vs. light tank lots of lead.